The gas turbine doubtlessly is one of the most important modern machines to convert energy from heat...

Informácie o knihe

Jazyk
Angličtina
Väzba
Kniha - Brožovaná
Vydalo
2015
Stránok
204
EAN
9783639761023
ISBN
3639761022
Enbook ID
09198060
Vydavateľ
Hmotnosť
304
Rozmery
152 x 229 x 12

Kompletný popis

The gas turbine doubtlessly is one of the most important modern machines to convert energy from heat to power, and improving its efficiency is a ceaseless task. The most practical route to increase the efficiency is to increase the maximum operating temperature. Over the past several decades, the improvement of this temperature was constantly attained by the developments of thermal barrier coating and superalloys, but almost reached a limit because the microstructural deterioration of both the base superalloy and the coating system due to the interdiffusion between them can be dramatically aggravated by further increasing temperature. The novel diffusion barrier type bond coat, therefore, is a solution to this issue. This book introduces how to form a rhenium-based diffusion barrier on a nickel-based superalloy. The formation process and thermal stability of the diffusion barrier are discussed through analyzing its macro- and micro-structures by XRD, EBSD, EPMA, SEM, and TEM, etc. This work provides the fundamental knowledge about the novel coating system, and should be especially useful to researchers and students in high-temperature materials science and technology.

Mohlo by vás zaujímať

Little Women

Louisa Alcott
9.82
25.94
81.58
199.94

Aberdeen-Angus Herd Book, Volume 22

Aberdeen-Angus Cattle Society
38.03
17.59
12.97
13.06

Our Hadeland Ancestors - Volume 2

Hadeland Lag Of America
26.14

Jo's Boys

Louisa May Alcott
15.62
3.33

Passing the Torch

Derek Gallop
13.56
41.08

Animal Farm

George Orwell
13.06

The Christmas Pig

Joanne K. Rowling
20.44
24.37
13.95

How To Walk

Thich Nhat Hanh
7.85

Zákazníci, ktorí si kúpili túto knihu, kúpili tiež

14.34

Sweet Home T02

Youngchan Hwang
19.95

Ženy za zády

Anna Stroganová
12.55

I-Inthanethi

Owen Jones
5.30
51.01

Neue Theorie der Erde

Georg Christoph Silberschlag
19.16
11.39
10.51
15.42

Wer ist Der?

Heidemarie Kunze
7.66